Powder grades, nominal chemical composition and properties of coatings

Grades Nominal composition Coating Hardness, HRC Properties
PG-S27

Fe C3.9 Cr26 Si 1.5 Ni1.7 W 0.3 Mo0.1 Mn1.1 ≥ 54.2

Resistance to abrasive wear at restrained load impacts and temperature max. 500 0C
PG-S1 Fe C2.9 Cr29 Si3.5 Mn1 Ni4 ≥ 54 Resistance to abrasive and gas-abrasive wear
PG-US25 Fe C4.9 Cr38 Si2.1 Ni1.4 Mn ≤ 2.5 ≥ 55.9 Resistance to intensive abrasive wear without impacts
PG-FBH6-2 Fe C4.5 Cr34 Si1.7 Mn2.7 B1.6 ≥ 53.2 Resistance to abrasive wear (deposition onto the equipment of  coal-mining industry)
PG-AN1 Fe C2.4 Cr29 Si2 Mn1 B1.5 ≥ 54 Resistance to abrasive wear at restrained load impacts (protective coatings for metallurgic equipment, agricultural technique, construction machinery etc.)
AP-FeCr30SiBNiCuAl Fe C4.9 Cr30 Si3.2 Ni1.4 Mn1 B2 Cu0.6 Al0.4 ≥ 60 Deposition of abrasive-resistant coatings onto the working components of agricultural machinery etc.
AP-FeCr18VNiMo (PN-AN2) Fe C Cr V Ni Mo Me 42-43, 51-53 at 650 0C Resistance to abrasive wear, tear and corrosion (protective coatings of polymers’ augers)
AP-FeNi15Cu7 Fe C2.6 Ni15 Cu7 Cr2.2 Si2.2 Mn1 240-200 HB Restoration of iron casting faults
AP-FeNiCr14Mo5WSiB Fe C1.4 Ni37 Cr14 Mo5 W4 Si2.5 B2.2 >35 Resistance to mechanical wear and corrosion, self-fluxing properties